Dry farming
Our company has many years of experience in drying oak wood.
We use the method of convective drying and press-vacuum.
In most cases, the convective drying chamber is used to dry lamella boards with a thickness of 30-55 mm, or blanks for the production of parquet.
The chamber has a volume of 120m3. The whole process is automated. A board with a thickness of 30 mm and an initial humidity of 60% is dried for 35-45 days. Thanks to gentle drying, the board comes out of the chamber flat and without cracks.
Press-vacuum drying is a certain know-how in the process of manufacturing lamellas. This chamber is designed to dry the lamella in a very short time of 13-17 hours, gives maximum flexibility in order fulfillment, allows you to save the lamella after drying without deformation, which allows you to save on the thickness of the raw lamella, and preserves the light, even color of the oak, which, in in turn, affects the grade of the lamella.


manufacturing
D r y f a r m i n g